This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2017, 8, 28–37, doi:10.3762/bjnano.8.4
Figure 1: MFM imaging of a HDD featuring PMR with magnetic domains being aligned parallel or antiparallel to ...
Figure 2: Magnetic recording medium: (a) TEM cross-section image with indication of the stack setup used for ...
Figure 3: Polarization dependence of absorptivity (λ = 785 nm): p-polarized light is 3.5–4 times better absor...
Figure 4: Influence of the DC bias field during laser illumination (λ = 532 nm, CW, P = 8 mW) on an as-is HDD...
Figure 5: (a) Free-hand writing of magnetic features at CW illumination (p-polarized, 785 nm, 12 mW), yieldin...
Figure 6: MFM phase scans and intensity profiles of “dots” laser-written at 785 nm. The laser power was kept ...
Figure 7: Power absorption per volume within the magnetic stack. (a) Cross-sectional absorption per layer of ...
Figure 8: Comsol thermal modelling of a Gaussian laser pulse (P = 40 mW; λ = 785 nm; τ = 50 ns, γ = 70°) bein...